Spring carbon and alloy steel bars. Specifications
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.72 | 0.80 | ||
Si | 0.17 | 0.37 | ||
Mn | 0.50 | 0.80 | ||
P | - | 0.035 | ||
S | - | 0.035 | ||
Cr | - | 0.25 | ||
Ni | - | 0.25 | ||
Cu | - | 0.20 |
Spring carbon and alloy steel bars. Specifications
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
519 (≥) | 218 (≥) | 22 | 44 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 142 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
526 (≥) | 716 (≥) | 31 | 41 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 442 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
564 | 478 | 536 |
We can customize the production of 75 grade, contact us for the best solution.