A 322 94L30 Stainless Steels to A 322 (2013)

A 322 94L30 - Specification & Application

  • A 322 (2013) - Steel Bars, Alloy, Standard Grades

Steel Bars, Alloy, Standard Grades

Chemical composition(wt.%) of A 322 94L30 grade: to A 322 (2013)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Si - 0.20
Mn - 0.30
P - -
S - -
Ni - 0.15
Cr 28.00 30.00
Al - -
Cu - 0.15
Ti - -
Fe - -
N - 0.02
Mo 3.50 4.20

A 322 94L30 - Detail

Steel Bars, Alloy, Standard Grades

Mechanical properties of grade A 322 94L30 A 322 (2013)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
741 (≥) 335 (≥) 21 12 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical properties of grade A 322 94L30 A 322 (2013)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
696 (≥) 259 (≥) 13 21 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 123
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
387 679 554

Equivalent Products

We can customize the production of A 322 94L30 grade, contact us for the best solution.