17-4PH Stainless Steels to SAE AMS 5342E (2006)

17-4PH - Specification & Application

  • SAE AMS 5342E (2006) - Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb (Nb) - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength (17-4)
  • SAE AMS 5343E (2006) - Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb (Nb) - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H1000) 150 ksi (1034 MPa) Tensile Strength (17-4)
  • SAE AMS 5344F (2007) - Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H900) 180 ksi (1241 MPa) Tensile Strength (17-4)
  • SAE AMS 5604G (2013) - Steel, Corrosion Resistant, Sheet, Strip, and Plate 16.5Cr - 4.0Ni - 4.0Cu - 0.30Cb Solution Heat Treated, Precipitation Hardenable
  • SAE AMS 5622F (2013) - Steel, Corrosion-Resistant, Bars, Wire, Forgings, Tubing, and Rings 16Cr - 4.0Ni - 0.30Cb - 4.0Cu Solution Heat Treated, Precipitation Hardenable Consumable Electrode Remelted
  • SAE AMS 5643/H1150 (2013) - Steel, Corrosion-Resistant, Bars, Wire, Forgings, Tubing and Rings 16Cr – 4.0Ni – 0.30Cb (Nb) – 4.0Cu Solution and Precipitation Heat Treated (H1150)
  • SAE AMS 5643S (2013) - Steel, Corrosion-Resistant, Bars, Wire, Forgings, Tubing, and Rings 16Cr - 4.0Ni - 0.30Cb - 4.0Cu Solution Heat Treated, Precipitation Hardenable

Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb (Nb) - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength (17-4)

Chemical composition(wt.%) of 17-4PH grade: to SAE AMS 5342E (2006)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.07
Si - 1.00
Mn - 1.00
Cr 15.00 17.50
Ni 3.00 5.00
Cu 3.00 5.00
Nb 0.15 1.45

17-4PH - Detail

SAE AMS 5342E (2006) Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb (Nb) - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength (17-4)
\
Used typically for parts requiring good corrosion resistance and strength up to 315°C.

Mechanical properties of grade 17-4PH SAE AMS 5342E (2006)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
234 (≥) 487 (≥) 34 42 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 231

Physical properties of grade 17-4PH SAE AMS 5342E (2006)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
877 (≥) 319 (≥) 32 41 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 212
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
753 723 434
We can customize the production of 17-4PH grade, contact us for the best solution.