Specification for Age-Hardening Stainless Steel Forgings
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.08 | ||
Mn | - | 1.00 | ||
Si | - | 1.00 | ||
P | - | 0.04 | ||
S | - | 0.03 | ||
Cr | 16.00 | 17.50 | ||
Ni | 6.00 | 7.50 | ||
Mo | - | - | ||
Al | - | 0.40 | ||
Ti | 0.40 | 1.20 |
Specification for Age-Hardening Stainless Steel Forgings
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
797 (≥) | 474 (≥) | 11 | 11 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 111 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
444 (≥) | 876 (≥) | 14 | 23 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 221 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
746 | 625 | 938 |
We can customize the production of SA-705 S17600 grade, contact us for the best solution.