A 270 TP316L Stainless Steels to A 270 (2010)

A 270 TP316L - Specification & Application

  • A 270 (2010) - Seamless and Welded Austenitic Stainless Steel Sanitary Tubing

Seamless and Welded Austenitic Stainless Steel Sanitary Tubing

Chemical composition(wt.%) of A 270 TP316L grade: to A 270 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.035
Cr 16.0 18.0
Ni 10.0 14.0
Mo 2.00 3.00
N - 0.10

A 270 TP316L - Detail

Seamless and Welded Austenitic Stainless Steel Sanitary Tubing

Mechanical properties of grade A 270 TP316L A 270 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
513 (≥) 545 (≥) 22 31 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical properties of grade A 270 TP316L A 270 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
147 (≥) 182 (≥) 43 44 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 124
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
675 294 998

Equivalent Products

We can customize the production of A 270 TP316L grade, contact us for the best solution.