S30815 Stainless Steels

S30815 - Specification & Application

Austenitic Chromium Nickel Silicon Heat Resisting Steel

Chemical composition(wt.%) of S30815 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.05 0.10
Si 1.40 2.00
Mn - 0.80
P - 0.04
S - 0.03
Cr 20.0 22.0
Ni 10.00 12.0
N 0.14 0.20
Ce 0.03 0.08

S30815 - Detail

Austenitic Chromium Nickel Silicon Heat Resisting Steel

Mechanical properties of grade S30815

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
439 (≥) 368 (≥) 42 13 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 233

Physical properties of grade S30815

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
594 (≥) 292 (≥) 31 32 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 443
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
948 999 257