SUS 304 Stainless Steels to G 4308 (2007)

SUS 304 - Specification & Application

  • G 4308 (2007) - Stainless steel wire rods

Stainless steel wire rods

Chemical composition(wt.%) of SUS 304 grade: to G 4308 (2007)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 18.00 20.00
Ni 8.00 10.50
Mo - -
N - -

SUS 304 - Detail

Stainless steel wire rods

Mechanical properties of grade SUS 304 G 4308 (2007)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
139 (≥) 368 (≥) 11 13 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 444

Physical properties of grade SUS 304 G 4308 (2007)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
895 (≥) 477 (≥) 31 22 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 331
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
582 151 521

Equivalent Products

We can customize the production of SUS 304 grade, contact us for the best solution.
sales@specificsteel.com