Specification for Single- or Double-Welded Austenitic Stainless Steel Pipe
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.08 | ||
Si | - | 1.00 | ||
Mn | 8.00 | 10.0 | ||
P | - | 0.06 | ||
S | - | 0.03 | ||
Cr | 19.0 | 21.0 | ||
Ni | 5.50 | 7.50 | ||
N | 0.15 | 0.40 |
SA-813 S21900
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
991 (≥) | 178 (≥) | 43 | 32 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 114 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
233 (≥) | 891 (≥) | 32 | 43 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 213 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
748 | 762 | 187 |