Cronifer 40 B
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
Ni | 36.0000 | 39.0000 | ||
Cr | 20.0000 | 23.0000 | ||
C | - | 0.1200 | ||
Mn | - | 1.0000 | ||
Si | 1.3000 | 2.2000 | ||
Al | - | 0.5000 | ||
La | 0.0300 | 0.2000 | ||
S | - | 0.0300 | ||
P | - | 0.0300 | ||
Cu | - | 0.5000 |
Cronifer 40 B
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
487 (≥) | 974 (≥) | 34 | 11 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 412 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
752 (≥) | 212 (≥) | 33 | 31 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 232 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
413 | 577 | 192 |
We can customize the production of Cronifer 40 B grade, contact us for the best solution.