Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.12 | 0.17 | ||
Si | 3.80 | 4.50 | ||
Mn | 0.50 | 1.00 | ||
P | - | 0.035 | ||
S | - | 0.030 | ||
Cr | 17.00 | 19.00 | ||
Ni | 11.00 | 13.00 | ||
Mo | - | 0.30 | ||
W | - | 0.20 | ||
Ti | 0.40 | 0.70 | ||
Al | 0.13 | 0.35 |
Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
395 (≥) | 583 (≥) | 12 | 12 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 213 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
492 (≥) | 799 (≥) | 12 | 33 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 432 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
182 | 576 | 183 |
We can customize the production of 15X18H12C4TЮ grade, contact us for the best solution.
–sales@specificsteel.com