ASTM501
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
c | 0.10 | - | ||
Si | - | 0.10 | ||
Mn | - | 0.10 | ||
P | - | 0.04 | ||
S | - | 0.03 | ||
Cr | 4.00 | 6.00 | ||
Mo | 0.40 | 0.65 |
ASTM501
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
589 (≥) | 241 (≥) | 21 | 31 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 344 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
745 (≥) | 265 (≥) | 43 | 34 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 141 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
272 | 218 | 941 |
We can customize the production of ASTM501 grade, contact us for the best solution.