G10214 Stainless Steels

G10214 - Specification & Application

Free cutting steel

Chemical composition(wt.%) of G10214 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 0.20
Mn - 0.50
P - -
S - -
Ni - remaining
Cr 15.00 17.00
Al 4.00 5.00
Cu - -
Ti - 0.50
Fe 2.00 4.00
N - -
Mo - 0.50
B - 0.006
Zr - 0.05

G10214 - Detail

Free cutting steel

Mechanical properties of grade G10214

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
397 (≥) 679 (≥) 43 34 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 231

Physical properties of grade G10214

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
468 (≥) 269 (≥) 44 13 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
876 235 626

Equivalent Products

We can customize the production of G10214 grade, contact us for the best solution.