Β2Φ Special Alloy

Chemical composition%of the ladle analysis of gradeΒ2Φ

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Ni(%)Mo(%)V(%)W(%)Cu(%)Ti(%)
1.05-1.220.10-0.400.15-0.45≤0.030≤0.0300.20-0.40≤0.35≤0.200.15-0.301.60-2.00≤0.30≤0.03

Mechanical properties of gradeΒ2Φ

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
246(≥) 218(≥) 42 21 11 Solution and Aging,Annealing,Ausaging,Q+T,etc 113

Physical properties of grade Β2Φ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
453(≥) 695(≥) 21 21 23 Solution and Aging,Annealing,Ausaging,Q+T,etc 344
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
227 627 288

Β2Φ Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

Β2Φ Steel Stock

Steel grade Dimension Shape Unit Quantity Delivery state Query
D2 Round bar Φ25-Φ380mm Round Bar Kgs 45325 Hot-Rolled+Annealed+black Enquiry
Cr12MoV 12-160(T)*310-610(W)*L Plate or Sheet Tons 12.38 Hot-Rolled+Annealed+black Enquiry
1.2601 12-160(T)*310-610(W)*L Plate or Sheet Tons 11.22 Hot-Rolled+Annealed+black Enquiry
IncoloyA-286 / GH 2132 Stock Φ8-65mm*L Round Bar Kgs 489 Hot-Rolled+Annealed+black Enquiry
X22CrMoV12-1 / 1.4923 Φ17mm Round Bar Kgs 300 Hot-Rolled+Annealed+black Enquiry
1.2083 Forged Plate T:105-185mm*W:510*L Plate or Sheet Tons 26 Forged+QT Enquiry
X22CrMoV12-1 / 1.4923 Φ30mm Round Bar Kgs 300 Hot-Rolled+Annealed+black Enquiry
1.4882 strip/sheet/plate stock 3.5x200x1000-2000mm Coil or Strip Kgs 200 Cold-Rolled+Annealed Enquiry
SA-437 Grade B4B/SUS 616 /422 Forged Bar Dia.160xL Round Bar Kgs 2120 Forged+QT Enquiry
1.2344(H13/X40CrMoV5-1/Z40CDV5) Stock List Dia.182mm - Dia.510mm Round Bar Tons 120 Forged+Annealed+black Enquiry
1.2344 ESR Round Bar Stock List(2019-9-3) Select 0 Select Enquiry
Stainless Steel 422 / Alloy 422 AMS 5655 UNS S42200/616/B4B Round Bar Stock Select 0 Select Enquiry
1.2343 ESR Stock list(2019-09-03) Select 0 Select Enquiry
1.2367 ESR Forged Round Bar stock(2019-09-03) Select 0 Select Enquiry
1.2379 ESR Round Bar Stock(2019-09-03) Select 0 Select Enquiry
1.2714 Hot-Work Mould Steel Flat Bar Stock(2019-09-03) Select 0 Select Enquiry
1.2714 Stock list 2020-06-15 Select 0 Select Enquiry
1.2344 Stock List 2020-06-15 Select 0 Select Enquiry
1.2714 QT Bar Stock List 2020-06-15 Select 0 Select Enquiry
1Cr11Ni2W2MoV,961,13Cr11Ni2W2MoV Sheet Select 0 Select Enquiry