Russia TY standard grades and chemical compositions of the high temperature alloy castings
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.11 | 0.16 | ||
Cr | 14.00 | 18.00 | ||
Al | 1.60 | 2.20 | ||
Mo | 3.00 | 4.50 | ||
Ti | 1.60 | 2.30 | ||
Co | - | - | ||
W | 4.50 | 6.50 | ||
Ni | - | remaining | ||
Nb | - | - | ||
Fe | - | 8.00 | ||
B | - | 0.02 | ||
Ce | - | - | ||
V | - | 0.30 | ||
Zr | - | - | ||
Mn | - | 0.60 | ||
Si | - | 0.60 | ||
S | - | 0.009 | ||
P | - | 0.015 |
Russia TY standard grades and chemical compositions of the high temperature alloy castings
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
254 (≥) | 733 (≥) | 41 | 12 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 233 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
841 (≥) | 733 (≥) | 14 | 21 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 422 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
993 | 776 | 768 |