09X14H19B2БP Stainless Steels

09X14H19B2БP - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 09X14H19B2БP grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.07 0.12
Si - 0.60
Mn - 2.00
P - 0.035
S - 0.020
Cr 13.00 15.00
Ni 18.00 20.00
Mo - 0.30
W 2.00 2.80
Ti - 0.20
Nb 0.90 1.30
B - 0.0050
Ce - 0.20

09X14H19B2БP - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 09X14H19B2БP

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
119 (≥) 939 (≥) 42 12 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 343

Physical properties of grade 09X14H19B2БP

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
714 (≥) 717 (≥) 23 24 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
521 625 681

Equivalent Products

We can customize the production of 09X14H19B2БP grade, contact us for the best solution.