1.3532, 16NiCrMo16-5 Structural Steel to EN ISO 683-17 (2014)

1.3532, 16NiCrMo16-5 - Specification & Application

  • EN ISO 683-17 (2014) - Heat-treated steels, alloy steels and free-cutting steels - Part 17: Ball and roller bearing steels (ISO 683-17:2014)

Heat-treated steels, alloy steels and free-cutting steels - Part 17: Ball and roller bearing steels (ISO 683-17:2014)

Chemical composition(wt.%) of 1.3532, 16NiCrMo16-5 grade: to EN ISO 683-17 (2014)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.14 0.18
Si - 0.40
Mn 0.25 0.55
P - 0.025
S - 0.015
Cr 1.00 1.40
Ni 3.80 4.30
Mo 0.20 0.30
Cu - 0.30
O - 0.002
Al - 0.05

1.3532, 16NiCrMo16-5 - Detail

1.3532, 16NiCrMo16-5

Mechanical properties of grade 1.3532, 16NiCrMo16-5 EN ISO 683-17 (2014)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
956 (≥) 532 (≥) 33 23 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 114

Physical properties of grade 1.3532, 16NiCrMo16-5 EN ISO 683-17 (2014)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
616 (≥) 973 (≥) 21 33 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 221
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
358 286 175

Equivalent Grade

Equivalent Products

We can customize the production of 1.3532, 16NiCrMo16-5 grade, contact us for the best solution.