15X6CЮ Stainless Steels

15X6CЮ - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 15X6CЮ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si 1.20 1.80
Mn - 0.50
P - 0.030
S - 0.025
Cr 5.50 7.00
Ni - 0.60
Mo - -
W - -
Ti - 0.20
Al 0.70 1.10

15X6CЮ - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 15X6CЮ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
747 (≥) 944 (≥) 34 34 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 434

Physical properties of grade 15X6CЮ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
838 (≥) 586 (≥) 31 33 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 144
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
198 833 798

Equivalent Grade

Equivalent Products

We can customize the production of 15X6CЮ grade, contact us for the best solution.