A 813 Grade TP 304N Stainless Steels to A 813/A 813M (2009)

A 813 Grade TP 304N - Specification & Application

  • A 813/A 813M (2009) - Single- or Double-Welded Austenitic Stainless Steel Pipe

Single- or Double-Welded Austenitic Stainless Steel Pipe

Chemical composition(wt.%) of A 813 Grade TP 304N grade: to A 813/A 813M (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 0.75
Mn - 2.00
P - 0.045
S - 0.03
Cr 18.0 20.0
Ni 8.00 10.5
N 0.10 0.16

A 813 Grade TP 304N - Detail

Single- or Double-Welded Austenitic Stainless Steel Pipe

Mechanical properties of grade A 813 Grade TP 304N A 813/A 813M (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
627 (≥) 789 (≥) 32 44 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 112

Physical properties of grade A 813 Grade TP 304N A 813/A 813M (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
729 (≥) 452 (≥) 32 12 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 443
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
551 443 894

Equivalent Products

We can customize the production of A 813 Grade TP 304N grade, contact us for the best solution.