1.0605 Structural Steel to DIN 17222 (1979)

1.0605 - Specification & Application

  • DIN 17222 (1979) - Cold Rolled Steel Strips for Springs; Technical Conditions of Delivery

Cold Rolled Steel Strips for Springs; Technical Conditions of Delivery

Chemical composition(wt.%) of 1.0605 grade: to DIN 17222 (1979)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.70 0.80
Si 0.15 0.35
Mn 0.60 0.80
P - 0.045
S - 0.045
Cr - -
Ni - -
Mo - -
Cu - -

1.0605 - Detail

Cold Rolled Steel Strips for Springs; Technical Conditions of Delivery

Mechanical properties of grade 1.0605 DIN 17222 (1979)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
711 (≥) 525 (≥) 11 22 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical properties of grade 1.0605 DIN 17222 (1979)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
862 (≥) 212 (≥) 23 32 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 442
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
152 171 224

Equivalent Grade

Equivalent Products

We can customize the production of 1.0605 grade, contact us for the best solution.
sales@specificsteel.com