F 880 Class A1-70 304L Stainless Steels to F 880M (2002)

F 880 Class A1-70 304L - Specification & Application

  • F 880M (2002) - Standard Specification for Stainless Steel Socket Set Screws (Metric)

Standard Specification for Stainless Steel Socket Set Screws (Metric)

Chemical composition(wt.%) of F 880 Class A1-70 304L grade: to F 880M (2002)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.030
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 18.00 20.00
Ni 8.00 12.0
N - 0.10

F 880 Class A1-70 304L - Detail

Standard Specification for Stainless Steel Socket Set Screws (Metric)

Mechanical properties of grade F 880 Class A1-70 304L F 880M (2002)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
774 (≥) 192 (≥) 31 32 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 341

Physical properties of grade F 880 Class A1-70 304L F 880M (2002)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
172 (≥) 158 (≥) 33 21 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 144
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
289 625 472
We can customize the production of F 880 Class A1-70 304L grade, contact us for the best solution.