F738 Class A1-50 S30500 Stainless Steels to F 738M (2002)

F738 Class A1-50 S30500 - Specification & Application

  • F 738M (2002) - Standard Specification for Stainless Steel Metric Bolts, Screws, and Studs

Standard Specification for Stainless Steel Metric Bolts, Screws, and Studs

Chemical composition(wt.%) of F738 Class A1-50 S30500 grade: to F 738M (2002)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.030
Cr 17.0 19.0
Ni 10.5 13.0

F738 Class A1-50 S30500 - Detail

Standard Specification for Stainless Steel Metric Bolts, Screws, and Studs

Mechanical properties of grade F738 Class A1-50 S30500 F 738M (2002)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
192 (≥) 164 (≥) 12 44 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical properties of grade F738 Class A1-50 S30500 F 738M (2002)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
941 (≥) 311 (≥) 34 12 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
242 831 722

Equivalent Products

We can customize the production of F738 Class A1-50 S30500 grade, contact us for the best solution.