H14 Tool Die Steels

H14 - Specification & Application

Hot-Work Tool Steel

Chemical composition(wt.%) of H14 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.35 0.45
Si 0.80 1.20
Mn 0.20 0.50
P - 0.030
S - 0.030
Cr 4.75 5.50
Mo - -
V - -
W 4.00 5.25
Ni+Cu - 0.75

H14 - Detail

Hot-Work Tool Steel

Mechanical properties of grade H14

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
548 (≥) 144 (≥) 44 44 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 244

Physical properties of grade H14

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
395 (≥) 385 (≥) 11 13 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 422
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
285 172 485

Equivalent Products

We can customize the production of H14 grade, contact us for the best solution.
sales@specificsteel.com