H14 Tool Die Steels

H14 - Specification & Application

Hot-Work Tool Steel

Chemical composition(wt.%) of H14 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.40
Si 0.20 0.40
Mn 0.20 0.40
Cr - 5.00
Mo - -
V - -
W - 5.00

H14 - Detail

Hot-Work Tool Steel

Mechanical properties of grade H14

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
112 (≥) 896 (≥) 34 13 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 234

Physical properties of grade H14

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
944 (≥) 951 (≥) 32 32 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
986 124 425

Equivalent Products

We can customize the production of H14 grade, contact us for the best solution.
sales@specificsteel.com