Chemical composition(wt.%) of SA-965 S30600 grade: to SA-965/SA-965M (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.018
Si 3.70 4.30
Mn - 2.00
P - 0.02
S - 0.02
Cr 17.0 18.5
Ni 14.0 15.5
Mo - 0.20
Cu - 0.50

SA-965 S30600 - Detail

Specification for Steel Forgings, Austenitic, for Pressure and High Temperature Parts

Mechanical properties of grade SA-965 S30600 SA-965/SA-965M (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
928 (≥) 465 (≥) 42 21 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 414

Physical properties of grade SA-965 S30600 SA-965/SA-965M (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
655 (≥) 283 (≥) 13 41 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 313
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
116 589 761