2326 Stainless Steels to SS 142326

2326 - Specification & Application

  • SS 142326 - Stainless steel - SS steel 2326

Stainless steel - SS steel 2326

Chemical composition(wt.%) of 2326 grade: to SS 142326

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.025
Si - 1.00
Mn - 0.50
P - 0.040
S - 0.020
Cr 17.00 19.00
Ni - 0.50
Mo 2.00 2.50
Ti 0.20+4(C+N) 0.80
N - 0.025

2326 - Detail

Stainless steel - SS steel 2326

Mechanical properties of grade 2326 SS 142326

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
137 (≥) 372 (≥) 34 23 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 221

Physical properties of grade 2326 SS 142326

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
966 (≥) 991 (≥) 31 31 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 431
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
449 697 651

Equivalent Grade

Equivalent Products

We can customize the production of 2326 grade, contact us for the best solution.