XH35BTЮ Stainless Steels

XH35BTЮ - Specification & Application

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Chemical composition(wt.%) of XH35BTЮ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 0.60
Mn - 0.60
P - 0.030
S - 0.020
Cr 14.00 16.00
Ni 33.00 37.00
Mo - -
Al 0.70 1.40
Ti 2.40 3.20
Fe - -
W 2.80 3.50
B - 0.020

XH35BTЮ - Detail

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Mechanical properties of grade XH35BTЮ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
786 (≥) 117 (≥) 43 33 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 421

Physical properties of grade XH35BTЮ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
477 (≥) 346 (≥) 23 13 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 223
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
192 321 924

Equivalent Grade

Equivalent Products