ЖC6K Stainless Steels

ЖC6K - Specification & Application

Russia TY standard grades and chemical compositions of the high temperature alloy castings

Chemical composition(wt.%) of ЖC6K grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.13 0.20
Cr 9.50 12.00
Al 5.00 6.00
Mo 3.50 4.80
Ti 2.50 3.20
Co 4.00 5.00
W 4.50 5.50
Ni - remaining
Nb - -
Fe - 2.00
B - 0.02
Ce - 0.015
V - -
Zr - -
Mn - 0.40
Si - 0.40
S - 0.015
P - 0.015
Pb - 0.001
Bi - 0.0005

ЖC6K - Detail

Russia TY standard grades and chemical compositions of the high temperature alloy castings

Mechanical properties of grade ЖC6K

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
759 (≥) 871 (≥) 34 33 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 142

Physical properties of grade ЖC6K

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
228 (≥) 644 (≥) 23 41 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 121
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
982 237 532

Equivalent Products

We can customize the production of ЖC6K grade, contact us for the best solution.