ЖC6K-BИ Stainless Steels

ЖC6K-BИ - Specification & Application

Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Chemical composition(wt.%) of ЖC6K-BИ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.13 0.20
Cr 9.50 12.00
Ni - remaining
Co 4.00 5.50
Mo 3.50 4.50
W 4.50 5.50
Al 5.00 6.00
Ti 2.50 3.20
Nb - -
Fe - 2.00

ЖC6K-BИ - Detail

Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Mechanical properties of grade ЖC6K-BИ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
292 (≥) 241 (≥) 11 32 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade ЖC6K-BИ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
882 (≥) 323 (≥) 23 14 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 241
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
541 312 789