09X16H15M3Б Stainless Steels

09X16H15M3Б - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 09X16H15M3Б grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.09
Si - 0.80
Mn - 0.80
P - 0.035
S - 0.020
Cr 15.00 17.00
Ni 14.00 16.00
Mo 2.50 3.00
W - 0.20
Ti - 0.20
Nb 0.60 0.90

09X16H15M3Б - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 09X16H15M3Б

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
756 (≥) 532 (≥) 41 11 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 221

Physical properties of grade 09X16H15M3Б

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
156 (≥) 398 (≥) 41 24 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 244
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
875 457 462

Equivalent Grade

Equivalent Products

We can customize the production of 09X16H15M3Б grade, contact us for the best solution.