Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Chemical composition(wt.%) of 10Xl1H20T2P(ЭИ696A) grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 1.00
Mn - 1.00
P - 0.020
S - 0.020
Cr 10.00 12.50
Ni 18.00 21.00
Mo - -
Al - 0.50
Ti 2.30 2.80
Fe - remaining
Cu - 0.20
B - 0.008

10Xl1H20T2P(ЭИ696A) - Detail

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Mechanical properties of grade 10Xl1H20T2P(ЭИ696A)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
461 (≥) 244 (≥) 14 31 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 244

Physical properties of grade 10Xl1H20T2P(ЭИ696A)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
713 (≥) 431 (≥) 31 21 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 341
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
466 941 161