A 732 Grade 14Q Stainless Steels to A 732/A 732M (2009)

A 732 Grade 14Q - Specification & Application

  • A 732/A 732M (2009) - Castings, Investment, Carbon and Low Alloy Steel for General Application, and Cobalt Alloy for High Strength at Elevated Temperatures

Castings, Investment, Carbon and Low Alloy Steel for General Application, and Cobalt Alloy for High Strength at Elevated Temperatures

Chemical composition(wt.%) of A 732 Grade 14Q grade: to A 732/A 732M (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 0.20
Mn - 0.50
P - -
S - -
Ni - remaining
Cr 15.00 17.00
Al 4.00 5.00
Cu - -
Ti - 0.50
Fe 2.00 4.00
N - -
Mo - 0.50
B - 0.006
Zr - 0.05

A 732 Grade 14Q - Detail

Castings, Investment, Carbon and Low Alloy Steel for General Application, and Cobalt Alloy for High Strength at Elevated Temperatures

Mechanical properties of grade A 732 Grade 14Q A 732/A 732M (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
547 (≥) 469 (≥) 34 14 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 241

Physical properties of grade A 732 Grade 14Q A 732/A 732M (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
377 (≥) 214 (≥) 12 14 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 342
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
816 887 682

Equivalent Products

We can customize the production of A 732 Grade 14Q grade, contact us for the best solution.