BЖЛ1-BИ Stainless Steels

BЖЛ1-BИ - Specification & Application

Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Chemical composition(wt.%) of BЖЛ1-BИ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.10 0.17
Cr 15.00 17.00
Ni - remaining
Co - -
Mo 3.50 5.00
W 2.00 2.50
Al 2.00 2.80
Ti 2.00 3.00
Nb - -
Fe 6.00 7.50

BЖЛ1-BИ - Detail

Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Mechanical properties of grade BЖЛ1-BИ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
513 (≥) 215 (≥) 22 11 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 432

Physical properties of grade BЖЛ1-BИ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
741 (≥) 611 (≥) 44 32 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 241
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
889 421 465

Equivalent Products

We can customize the production of BЖЛ1-BИ grade, contact us for the best solution.
sales@specificsteel.com