BЖЛ18-BИ Stainless Steels

BЖЛ18-BИ - Specification & Application

Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Chemical composition(wt.%) of BЖЛ18-BИ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
Si - 0.40
Mn - 0.40
P - 0.015
S - 0.015
B - 0.06
Ce - 0.02
Zr - 0.02
Y - -
Pb - 0.001
Bi - 0.0005

BЖЛ18-BИ - Detail

Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Mechanical properties of grade BЖЛ18-BИ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
922 (≥) 328 (≥) 42 11 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 243

Physical properties of grade BЖЛ18-BИ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
264 (≥) 668 (≥) 13 31 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
984 912 598

Equivalent Products

We can customize the production of BЖЛ18-BИ grade, contact us for the best solution.