BЖЛ2-BИ Stainless Steels

BЖЛ2-BИ - Specification & Application

Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Chemical composition(wt.%) of BЖЛ2-BИ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
Si 1.00 2.00
Mn - -
P - -
S - 0.02
B - 0.015
Ce - -
Zr - -
Y - -
Pb - -
Bi 2.00 3.50

BЖЛ2-BИ - Detail

Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Mechanical properties of grade BЖЛ2-BИ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
675 (≥) 544 (≥) 33 12 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade BЖЛ2-BИ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
967 (≥) 515 (≥) 13 14 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 431
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
798 459 362

Equivalent Products

We can customize the production of BЖЛ2-BИ grade, contact us for the best solution.