B-4 Stainless Steels to SAE AMS T 9046 (2002)

B-4 - Specification & Application

  • SAE AMS T 9046 (2002) - Titanium and Titanium Alloy, Sheet, Strip, and Plate

Titanium and Titanium Alloy, Sheet, Strip, and Plate

Chemical composition(wt.%) of B-4 grade: to SAE AMS T 9046 (2002)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Si - 0.05
Mn - 1.50
P - 0.04
S - 0.01
Ni - remaining
Cr 0.50 1.50
Al 0.10 0.50
Cu - 0.50
Ti - -
Fe 1.00 6.00
Mo 26.00 30.00
Co - 2.50

B-4 - Detail

Titanium and Titanium Alloy, Sheet, Strip, and Plate

Mechanical properties of grade B-4 SAE AMS T 9046 (2002)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
722 (≥) 195 (≥) 41 23 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 111

Physical properties of grade B-4 SAE AMS T 9046 (2002)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
179 (≥) 225 (≥) 24 22 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 221
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
381 945 357

Equivalent Products

We can customize the production of B-4 grade, contact us for the best solution.