B 569 C26130 Stainless Steels to B 569 (2009)

B 569 C26130 - Specification & Application

  • B 569 (2009) - Brass Strip in Narrow Widths and Light Gage for Heat-Exchanger Tubing

Brass Strip in Narrow Widths and Light Gage for Heat-Exchanger Tubing

Chemical composition(wt.%) of B 569 C26130 grade: to B 569 (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Si - 0.75
Mn - 0.75
P - -
S - -
Ni - 0.50
Cr 25.00 27.00
Al - -
Cu - 0.20
Ti - -
Fe - -
N - 0.04
Mo 0.75 1.50

B 569 C26130 - Detail

Brass Strip in Narrow Widths and Light Gage for Heat-Exchanger Tubing

Mechanical properties of grade B 569 C26130 B 569 (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
216 (≥) 326 (≥) 32 23 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 314

Physical properties of grade B 569 C26130 B 569 (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
568 (≥) 312 (≥) 32 33 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 141
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
337 299 528