16X11H282MΦ Stainless Steels

16X11H282MΦ - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 16X11H282MΦ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.14 0.18
Si - 0.60
Mn - 0.60
P - 0.030
S - 0.025
Cr 10.50 12.00
Ni 1.40 1.80
Mo 0.35 0.50
W 1.60 2.00
Ti - 0.20
V 0.18 0.30

16X11H282MΦ - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 16X11H282MΦ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
138 (≥) 358 (≥) 12 22 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 231

Physical properties of grade 16X11H282MΦ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
199 (≥) 574 (≥) 22 43 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 443
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
532 181 336

Equivalent Grade

Equivalent Products

We can customize the production of 16X11H282MΦ grade, contact us for the best solution.