A 314 S33228 Stainless Steels to A 314 (2008)

A 314 S33228 - Specification & Application

  • A 314 (2008) - Stainless Steel Billets and Bars for Forging

Stainless Steel Billets and Bars for Forging

Chemical composition(wt.%) of A 314 S33228 grade: to A 314 (2008)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.08
Mn - 1.00
Si - 0.30
P - 0.02
S - 0.015
Cr 26.0 28.0
Ni 31.0 33.0
Ce 0.05 0.10
Nb 0.10 1.00
Al - 0.025

A 314 S33228 - Detail

Stainless Steel Billets and Bars for Forging

Mechanical properties of grade A 314 S33228 A 314 (2008)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
993 (≥) 881 (≥) 42 23 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical properties of grade A 314 S33228 A 314 (2008)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
426 (≥) 815 (≥) 34 41 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 234
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
915 337 811

Equivalent Products

We can customize the production of A 314 S33228 grade, contact us for the best solution.