A 632 S31000 Stainless Steels to A 632 (2009)

A 632 S31000 - Specification & Application

  • A 632 (2009) - Seamless and Welded Austenitic Stainless Steel Tubing (Small-Diameter) for General Service

Seamless and Welded Austenitic Stainless Steel Tubing (Small-Diameter) for General Service

Chemical composition(wt.%) of A 632 S31000 grade: to A 632 (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.25
Si - 1.50
Mn - 2.00
P - 0.045
S - 0.03
Cr 24.00 26.00
Ni 19.00 22.00
Mo - 1.00
Cu - 1.00

A 632 S31000 - Detail

Seamless and Welded Austenitic Stainless Steel Tubing (Small-Diameter) for General Service

Mechanical properties of grade A 632 S31000 A 632 (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
375 (≥) 879 (≥) 24 11 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 141

Physical properties of grade A 632 S31000 A 632 (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
117 (≥) 547 (≥) 33 31 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 443
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
162 715 132
We can customize the production of A 632 S31000 grade, contact us for the best solution.