201L Stainless Steels to A 213/A 213M (2011)

201L - Specification & Application

  • A 213/A 213M (2011) - Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Chemical composition(wt.%) of 201L grade: to A 213/A 213M (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.75
Mn 5.05 7.50
P - 0.045
S - 0.03
Cr 16.0 18.0
Ni 3.50 5.50
N - 0.25

201L - Detail

Stainless and heat resisting steels

A 213/A 213M (2011) Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Mechanical properties of grade 201L A 213/A 213M (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
345 (≥) 761 (≥) 11 32 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 423

Physical properties of grade 201L A 213/A 213M (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
132 (≥) 142 (≥) 11 31 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 214
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
387 313 618