BЖЛ12Э-BИ Stainless Steels

BЖЛ12Э-BИ - Specification & Application

Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Chemical composition(wt.%) of BЖЛ12Э-BИ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.12 0.20
Cr 8.50 10.00
Ni - remaining
Co 8.00 10.00
Mo 2.70 3.40
W 1.00 1.80
Al 5.00 5.70
Ti 4.20 4.70
Nb 0.50 1.00
Fe - 2.00

BЖЛ12Э-BИ - Detail

Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Mechanical properties of grade BЖЛ12Э-BИ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
556 (≥) 555 (≥) 42 12 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade BЖЛ12Э-BИ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
142 (≥) 167 (≥) 33 24 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 244
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
197 138 223

Equivalent Products

We can customize the production of BЖЛ12Э-BИ grade, contact us for the best solution.