BЖЛ12y Stainless Steels

BЖЛ12y - Specification & Application

Russia TY standard grades and chemical compositions of the high temperature alloy castings

Chemical composition(wt.%) of BЖЛ12y grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.14 0.20
Cr 8.50 10.50
Al 5.00 5.70
Mo 2.70 3.40
Ti 4.20 4.70
Co 12.00 15.00
W 1.00 1.80
Ni - remaining
Nb 0.50 1.00
Fe - 2.00
B - 0.015
Ce - 0.02
V 0.50 1.00
Zr - 0.02
Mn - 0.40
Si - 0.40
S - 0.015
P - 0.015

BЖЛ12y - Detail

Russia TY standard grades and chemical compositions of the high temperature alloy castings

Mechanical properties of grade BЖЛ12y

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
451 (≥) 994 (≥) 42 11 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 311

Physical properties of grade BЖЛ12y

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
611 (≥) 686 (≥) 11 33 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 321
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
292 653 492