BЖЛ14H-BИ Stainless Steels

BЖЛ14H-BИ - Specification & Application

Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Chemical composition(wt.%) of BЖЛ14H-BИ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.03 0.08
Cr 18.00 20.00
Ni - remaining
Co - -
Mo 4.00 5.00
W - -
Al 1.20 1.50
Ti 2.50 2.90
Nb 1.80 2.80
Fe 8.00 10.00

BЖЛ14H-BИ - Detail

Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Mechanical properties of grade BЖЛ14H-BИ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
962 (≥) 346 (≥) 32 14 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 434

Physical properties of grade BЖЛ14H-BИ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
319 (≥) 517 (≥) 12 21 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 243
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
429 263 412

Equivalent Products

We can customize the production of BЖЛ14H-BИ grade, contact us for the best solution.