CДП1-4 Stainless Steels

CДП1-4 - Specification & Application

Russia TY standard high temperature oxidation the chemical composition of casting alloy rod

Chemical composition(wt.%) of CДП1-4 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
Ni - remaining
Co 6.00 8.00
Cr 19.00 22.00
Al 11.00 13.00
Y 0.20 0.60
C - 0.05
Fe - 0.30
Si - 0.20
Cu - 0.05
O、N、H - 0.02

CДП1-4 - Detail

Russia TY standard high temperature oxidation the chemical composition of casting alloy rod

Mechanical properties of grade CДП1-4

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
648 (≥) 171 (≥) 31 42 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 233

Physical properties of grade CДП1-4

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
829 (≥) 172 (≥) 21 31 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
821 987 455

Equivalent Grade

Equivalent Products

We can customize the production of CДП1-4 grade, contact us for the best solution.