Marage 300 Stainless Steels to SAE AMS 6463E (2013)

Marage 300 - Specification & Application

  • SAE AMS 6463E (2013) - Wire, Steel Welding, 18.5Ni - 8.5Co - 5.2Mo - 0.72Ti - 0.10Al, (Marage 300), Vacuum Melted, Environment Controlled Packaging

Wire, Steel Welding, 18.5Ni - 8.5Co - 5.2Mo - 0.72Ti - 0.10Al, (Marage 300), Vacuum Melted, Environment Controlled Packaging

Chemical composition(wt.%) of Marage 300 grade: to SAE AMS 6463E (2013)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.10
Mn - 0.10
Ni - 18.00
Cr - -
Al - 0.10
Cu - -
Ti - 0.40
Fe - -
Mo - 5.00
Co - 8.00

Marage 300 - Detail

Wire, Steel Welding, 18.5Ni - 8.5Co - 5.2Mo - 0.72Ti - 0.10Al, (Marage 300), Vacuum Melted, Environment Controlled Packaging

Mechanical properties of grade Marage 300 SAE AMS 6463E (2013)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
993 (≥) 414 (≥) 11 43 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 242

Physical properties of grade Marage 300 SAE AMS 6463E (2013)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
396 (≥) 589 (≥) 34 31 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 144
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
461 576 279

Equivalent Products

We can customize the production of Marage 300 grade, contact us for the best solution.