W43070 Stainless Steels

W43070 - Specification & Application

Composite thermal spray wire (CW-FeCr-4)

Chemical composition(wt.%) of W43070 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn 3.75 4.75
P - 0.045
S - 0.03
Ni 9.00 10.50
Cr 19.00 22.00
Al - -
Cu - -
Ti - -
Fe - -
N - -
Mo - -
V - -

W43070 - Detail

Composite thermal spray wire (CW-FeCr-4)

Mechanical properties of grade W43070

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
518 (≥) 325 (≥) 44 33 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical properties of grade W43070

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
392 (≥) 252 (≥) 32 31 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
496 932 248