XH51BMTЮ/KΦK-BД Stainless Steels

XH51BMTЮ/KΦK-BД - Specification & Application

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Chemical composition(wt.%) of XH51BMTЮ/KΦK-BД grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 0.035
Mn - 0.03
P - -
S - -
Cr 9.00 12.00
Ni - remaining
Mo 5.00 7.00
Al 3.90 4.80
Ti 2.20 2.90
Fe - 3.00
Co 14.00 15.50
W 5.00 6.50
V 0.20 0.80
B - 0.002

XH51BMTЮ/KΦK-BД - Detail

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Mechanical properties of grade XH51BMTЮ/KΦK-BД

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
235 (≥) 467 (≥) 14 34 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 414

Physical properties of grade XH51BMTЮ/KΦK-BД

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
397 (≥) 793 (≥) 34 43 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 341
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
619 214 383