PH 13-8Mo Stainless Steels to SAE AMS 5840E (2010)

PH 13-8Mo - Specification & Application

  • SAE AMS 5840E (2010) - Steel, Corrosion and Heat Resistant, Welding Wire 13Cr - 8.0Ni - 2.3Mo - 1.1Al Vacuum Melted

Steel, Corrosion and Heat Resistant, Welding Wire 13Cr - 8.0Ni - 2.3Mo - 1.1Al Vacuum Melted

Chemical composition(wt.%) of PH 13-8Mo grade: to SAE AMS 5840E (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - -
Mn - -
Cr 12.25 13.25
Ni 7.50 8.50
Mo 2.00 2.50
Co - -
W - -
Al 0.90 1.35
Cu - -
Ti - -
Fe - -

PH 13-8Mo - Detail

Steel, Corrosion and Heat Resistant, Welding Wire 13Cr - 8.0Ni - 2.3Mo - 1.1Al Vacuum Melted

Mechanical properties of grade PH 13-8Mo SAE AMS 5840E (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
331 (≥) 497 (≥) 32 42 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical properties of grade PH 13-8Mo SAE AMS 5840E (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
993 (≥) 187 (≥) 12 14 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 324
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
653 429 681
We can customize the production of PH 13-8Mo grade, contact us for the best solution.