S41000 Stainless Steels

S41000 - Specification & Application

Martensitic Chromium Stainless Steel (Hardenable by Heat Treatment)

Chemical composition(wt.%) of S41000 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn - 1.00
Si - 1.00
P - 0.04
S - 0.03
Cr 11.50 13.50
Ni - -
Mo - -

S41000 - Detail

Martensitic Chromium Stainless Steel (Hardenable by Heat Treatment)

Mechanical properties of grade S41000

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
977 (≥) 591 (≥) 14 42 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical properties of grade S41000

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
968 (≥) 218 (≥) 41 32 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 222
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
917 222 541
We can customize the production of S41000 grade, contact us for the best solution.