SA-789 S31803 Stainless Steels to SA-789/SA-789M

SA-789 S31803 - Specification & Application

  • SA-789/SA-789M - Specification for Seamless and Welded Ferritic /Austenitic Stainless Steel Tubing for General Service

Specification for Seamless and Welded Ferritic /Austenitic Stainless Steel Tubing for General Service

Chemical composition(wt.%) of SA-789 S31803 grade: to SA-789/SA-789M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 2.00
Si - 1.00
P - 0.03
S - 0.02
Cr 21.00 23.00
Ni 4.50 6.50
Mo 2.50 3.50
N 0.08 0.20

SA-789 S31803 - Detail

Specification for Seamless and Welded Ferritic /Austenitic Stainless Steel Tubing for General Service

Mechanical properties of grade SA-789 S31803 SA-789/SA-789M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
896 (≥) 986 (≥) 22 23 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 234

Physical properties of grade SA-789 S31803 SA-789/SA-789M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
548 (≥) 555 (≥) 24 32 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 313
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
415 539 678

Equivalent Products

We can customize the production of SA-789 S31803 grade, contact us for the best solution.
sales@specificsteel.com